1Radis, Rene ; Zickler, Gerald ; Stockinger, M ; Sommitsch, Christof ; Kozeschnik, Ernst Interaction of the Precipitation Kinetics of Delta and Gamma Prime Phases in Nickel-Base Superalloy ATI Allvac 718 PlusKonferenzbeitrag Inproceedings2009